Description
In terms of chemical composition, CK75 contains 0.70-0.80% carbon, 0.60-0.80% manganese, and 0.15-0.35% silicon, which contribute to its hardness and strength. Additionally, it has a tensile strength ranging from 750 to 950 MPa and is capable of undergoing heat treatment, making it ideal for applications requiring high wear resistance
| Grade | CK75 |
| Material No | 1/1248 |
| C | 0.70-0.80 |
| Si | 0.15-0.35 |
| Mn | 0.60-0.90 |
| Cr | MAX 0.40 |
| P | MAX 0.025 |
| S | MAX 0.025 |
| Ni | MAX 0.40 |
| Cu | – |
| Other | MO≤ 0.1 |